| Aesculus octandra | |||||
| Family: Hippocastanaceae | |||||
| Yellow Buckeye | |||||
The genus Aesculus contains 13 species, which grow in the United States [6], Mexico [1] and Eurasia [6]. Species cannot be separated based on microanatomy. The name aesculus is a Latin name of a European oak or other mast-bearing tree.
Aesculus californica-California buckeye, horsechestnut
Aesculus glabra*-American horsechestnut, buckeye, fetid buckeye, Ohio buckeye, sevenleaf buckeye, smooth buckeye, sticking buckeye, stinking buckeye, Texas buckeye, white buckeye
Aesculus glabra var. glabra-Ohio buckeye (typical)
Aesculus glabra var. arguta-Texas buckeye, white buckeye
Aesculus hippocastanum-buckeye, common horsechestnut, conker-tree, European horsechestnut, horse chestnut (Europe)
Aesculus octandra*-big buckeye, buckeye, large buckeye, Ohio buckeye, sweet buckeye, yellow buckeye
Aesculus parviflora-bottlebrush buckeye, shrubby buckeye
Aesculus pavia-buckeye, firecracker plant, red buckeye, red-flowered buckeye, red pavia, scarlet buckeye, woolly, woolly buckeye
Aesculus sylvatica-dwarf buckeye, Georgia buckeye, painted buckeye
*commercial species
Distribution
In the United States, buckeye ranges from the Appalachians of Pennsylvania, Virginia, and North Carolina westward to Kansas, Oklahoma, and Texas. Buckeye is not customarily separated from other species when manufactured into lumber and can be utilized for the same purposes as aspen, basswood, and sap yellow-poplar. The following description is for yellow buckeye (Aesculus octandra).
The Tree
Buckeye is a tree 30 to 70 ft (9 to 21 m) high and 2 ft (0.6 m) in diameter. It grows best in rich moist soil along the banks of streams and in river bottoms. Buckeye matures in 60 to 80 years. It is one of the initial trees to leaf-out in the spring. The twigs have a foul odor when broken.
The Wood
General
The white sapwood of buckeye merges gradually into the creamy or yellowish white heartwood. The wood is uniform in texture, generally straight-grained, light in weight, weak when used as a beam, soft, and low in shock resistance. It is rated low on machinability such as shaping, mortising, boring, and turning. The centers of logs can be discolored to grayish brown, due to a sapstain fungus.
Mechanical Properties (2-inch standard)
|
|
||||||||
|
gravity |
x106 lbf/in2 |
lbf/in2 |
lbf/in2 |
lbf/in2 |
in-lbf/in3 |
lbf |
lbf/in2 |
|
| Green |
|
|
|
|
|
|
|
|
| Dry |
|
|
|
|
|
|
|
|
| aWML = Work to maximum load.
Reference (59). |
||||||||
Drying and Shrinkage
| Type of shrinkage |
(green to final moisture content) |
||
|
|
|
|
|
| Tangential |
|
|
|
| Radial |
|
|
|
| Volumetric |
|
|
|
| References: 0% MC (98), 6% and 20% MC (90). |
|||
Kiln Drying Schedulesa
|
|
|||||
| Condition |
|
|
|
|
|
| Standard |
|
|
|
|
|
| aReferences (6, 86). | |||||
Working Properties: No information available at this time.
Durability: Rated as slightly or nonresistant to heartwood decay.
Preservation: No information available at this time.
Uses: Furniture, artificial limbs, splints, boxes and crates, caskets and coffins, paper pulp, signs, trunks, valises, scientific instruments, wooden ware, novelties, food containers, strips woven into summer hats, and planing mill products.
Toxicity: The nuts and twigs are poisonous, containing aescin, a cytotoxin (54).
Additional Reading and References Cited (in parentheses)
6. Boone, R.S.; Kozlik, C.J.; Bois, P.J.; Wengert, E.M. 1988. Dry kiln schedules for commercial woodstemperate and tropical. Gen. Tech. Rep. FPLGTR57. Madison, WI: U.S. Department of Agriculture, Forest Service, Forest Products Laboratory.
9. Brown, H.P.; Panshin, A.J. 1940. Commercial timbers of the United States, their structure, identification, properties and uses. New York: McGrawHill Book Co.
19. Collingwood, G.H. 1938. Ohio buckeye. American Forests. July.
24. Davis, E.M. 1942. Machining and related characteristics of southern hardwoods. Tech. Bull. 324. Washington, DC: U.S. Department of Agriculture, Forest Service.
27. Duff, J.E. 1973. Buckeye, an American wood. FS222. Washington, DC: U.S.
Department of Agriculture, Forest Service.
29. Elias, T.S. 1980. The complete trees of North America, field guide and natural history. New York: van Nostrand Reinhold Company.
35. Gibson, H. 1913. American forest trees. Hardwood Record.
37. Harlow, W.M.; Harrar, E.S. 1950. Textbook of dendrology, covering the important forest trees of the United States and Canada. New York: McGrawHill Book Company.
51. Koehler, A. 1917. Guidebook for the identification of woods used for ties and timbers. Washington, DC: U.S. Department of Agriculture, Forest Service.
54. Lampe, K.F.; McCann, M.A. 1985. AMA handbook of poisonous and injurious plants. Chicago, IL: American Medical Association.
55. Little, Jr., E.L. 1979. Checklist of United States trees (native and naturalized). Agric. Handb. 541. Washington, DC: U.S. Department of Agriculture, Forest Service. U.S. Government Printing Office.
59. Markwardt, L.J.; Wilson, T.R.C. 1935. Strength and related properties of woods grown in the United States. Tech. Bull. 479. Washington, DC: U.S. Department of Agriculture, Forest Service. U.S. Government Printing Office.
66. Nellis, J.C. 1918. Lumber used in the manufacture of wooden products. Bull. 605. Washington, DC: U.S. Department of Agriculture, Forest Service.
68. Panshin, A.J.; de Zeeuw, C. 1980. Textbook of wood technology, 4th ed. New York: McGrawHill Book Co..
74. Record, S.J.; Hess R.W. 1943. Timbers of the new world. New Haven, CT: Yale
University Press.
79. Sargent, C.S. 1905. Manual of the trees of North America. New York: Houghton,
Mifflin and Co.
86. Simpson, W.T. 1991. Dry kiln operator's manual. Ag. Handb. 188. Madison, WI: U.S. Department of Agriculture, Forest Service, Forest Products Laboratory.
90. Summitt, R.; Sliker, A. 1980. CRC handbook of materials science. Boca Raton, FL: CRC Press, Inc. Vol. 4.
98. U.S. Department of Agriculture. 1987. Wood handbook: wood as an engineering material. Agric. Handb. 72. (Rev.) Washington, DC: U.S. Department of Agriculture. 466 p.